Ni-Cr-Fe Filler Metal
INCONEL Filler Metal 92 is used for gas-tungsten-arc and gas-metal-arc welding of austenitic and ferritic steels and nickel alloys. Applications include joining INCONEL and INCOLOY alloys to stainless steels, carbon steels, and MONEL alloys; joining MONEL alloys and Nickel 200 to stainless steels; and joining stainless steels to carbon steels. The filler metal is also used for welding nickel steels. The high Ti concentration provides excellent porosity resistance in field welding applications.
INCONEL Filler Metal 92 provides high strength and corrosion resistance at temperatures ranging from the cryogenic region to over 1800°F (980°C). Weld deposits can be age hardened for greater strength at temperatures to about 1300°F (700°C).
Specifications
AWS A5.14 ERNiCrFe-6 (UNS N07092)
ASME II, Part C, SFA-5.14, ERNiCrFe-6 (UNS N07092)
ASME IX, F-No.43
*BS 2901 NA39
*(EN) ISO 18274 – SNi 7092 (NiCr15Ti3Mn)
*Supply to these specifications available upon request.
For manufacture to ASME III NCA3800, NB2400, MIL, Rolls Royce, AMS and other specifications please refer your inquiry to the Technical Department prior to order placement.
Approvals
Please confirm details of current scope of approvals with the Technical Department prior to order placement.
| Limiting Chemical Composition | |||
|---|---|---|---|
| Ni+Co: | 67.0 min. | Cu: | 0.50 max. |
| C: | 0.08 max. | Cr: | 14.0-17.0 |
| Mn: | 2.0-2.7 | Ti: | 2.5-3.5 |
| Fe: | 8.0 max. | P: | 0.03 max. |
| S: | 0.015 max. | Others: | 0.50 max. |
| Si: | 0.35 max. | ||
| Minimum Mechanical Properties (As Welded) | |
|---|---|
| Tensile Strength, psi | 80,000 |
| MPa | 552 |
| Elongation, (4d) % | 30 |
| Available Product Forms | ||||||||
|---|---|---|---|---|---|---|---|---|
| mm | 0.8 | 0.9 | 1.0 | 1.14 | 1.2 | 1.6 | 2.4 | 3.2 |
| in | 0.030 | 0.035 | 0.040 | 0.045 | 0.047 | 0.062 | 0.093 | 0.125 |