INCONEL® Filler Metal 718

Ni-Fe-Cr Filler Metal

INCONEL Filler Metal 718 is used for gas-tungsten-arc welding of INCONEL alloys 718,
706 and X-750. The weld metal is age hardenable and has mechanical properties
comparable to those of the base metals.

Specifications
AWS A5.14 ERNiFeCr-2 (UNS N07718)
ASME II, Part C, SFA-5.14, ERNiFeCr-2 (UNS N07718)
*BS2901 NA 51
*DIN 1736 SG-NiCr19NbMoTi (2.4667)
*(EN) ISO 18274 – SNi7718 (NiFe19Cr19Nb5Mo3)
*Supply to these specifications available upon request.
For manufacture to ASME III (NCA3800, NB2400), Rolls Royce, AMS and other specifications please refer your inquiry to the Technical Department prior to order placement.

Approvals
Please confirm details of current scope of approvals with the Technical Department prior to order placement.

Limiting Chemical Composition
Ni:50.0-55.0Al:0.20-0.80
C: 0.08 max.Ti:0.65-1.15
Mn:0.35 max.Nb+Ta:4.75-5.50
Fe:RemainderMo:2.80-3.30
S:0.015 max.P:0.015 max.
Si:0.35 max.B:0.006 max.
Cu:0.30 max.Co:1.0 max.
Cr:17.0-21.0
Minimum Mechanical Properties
Tensile Strength, psi165,000
MPa1138
Properties
(Age hardened condition: 1325°F (720°C)/8 hours, Furnace Cool 100°F (55°C)/hour to 1150°F (620°C)/8 hours, Air Cool)
Available Product Forms
mm0.80.91.01.141.21.62.43.2
in0.0300.0350.0400.0450.0470.0620.0930.125
Filler metals available on spool and in cut straight lengths.Straight Lengths – 915 mm (36 in.)